WOCA RP 2K instructions

It is important that both wood and finish have a temperature of min. 59°F (preferably around 68°F) and air humidity of approx. 50%. The room must be well-ventilated for optimal evaporation and drying time. For the final sanding to bare wood, use grit 120-150 sandpaper. Vacuum thoroughly and tack the floor. The floor should be completely dry before application of WOCA RP 2K

Always remember to test on a less visible spot to check the compatibility of the surface with the product.

  1. Mix WOCA 2K hardener with the WOCA RP 2K Finish and shake thoroughly before use. Leave the mixture to stand for ten minutes before use, to allow the hardener to activate.
  2. Apply the 1st coat of the mixture with a paint roller and leave the floor to dry for 2-3 hours.
  3. Apply the 2nd coat and leave the surface to dry until the next day.
  4. Sand the surface with 120-150 and vacuum clean the surface thoroughly.
  5. Apply the 3rd/final coat of WOCA RP 2K with the freshly mixed hardener added.

Pot life: The mixture must be used within 48 hours. Shake/stir thoroughly before use.  Mixing ratio of hardener to finish: 1:1

Dry time between coats: 2-3 hours at 68°F

After the final coat the floor can being walked on with caution after 24 hours at 68°F

Wait 3 days before putting furniture on the floor. Wait 8 days before laying rugs and cleaning the floor.

Fully hardened /cured: 8 days at 68°F